One page. Drape weight, FR rating, recertification window. Print it, laminate it, tape it to the fly rail. The fabric inventory you have to work with on a load-in is what's already in the venue - this reference helps you read it quickly.

Typical theatre drape fabric weights

Weights below are per square metre at standard width. Use them to estimate handling weight before you lift a drape onto a batten. Always check the actual maker's tag where it survives - older stock varies.

Fabric Weight per m² Typical use Light-tight?
Wool serge (heavy)540 g/m²Tabs, legs, bordersYes
Wool serge (medium)440 g/m²Legs, bordersYes
FR-treated cotton velour620 g/m²House tabs, formal maskingYes
FR-treated cotton duvetyne340 g/m²Masking, blackoutYes
Cotton scrim (sharkstooth)100 g/m²Reveal effects, gauzeNo (lit from front)
Cotton filled cloth250 g/m²Cyclorama, lit backdropPartial
Nessel canvas (painted backdrops)200 g/m²Scenic painting, painted backdropsPartial
FR polyester (printed backdrops)Varies by baseDigitally printed scenicPartial

FR ratings - what to look for on the tag

In Australia the relevant standard is AS 1530. A maker's tag should show:

  • Standard referenced - AS 1530 at minimum.
  • Date of certification.
  • Treatment type - inherently FR (woven from FR fibre) or topically FR-treated (chemical applied to a non-FR base fabric).
  • Recertification interval if topically treated, usually 4 to 5 years.

Recertification windows

Recertification is not the same as retreatment. The certificate window below is how long a treatment stays valid on paper. The retreatment cycle is shorter - plan on 2-3 years, sooner for drapes that are washed, handled hard or hung in daylight.

Drape type Recertify every Trigger for early retest
Inherently FR (Trevira CS, FR polyester)Not required, permanentVisible char, smoke damage, fire exposure
Topically FR-treated (wool serge, cotton velour)4 to 5 yearsAny wet cleaning, water damage, fire exposure
FR-treated canvas or painted backdrops4 to 5 yearsAny wet cleaning, repainting, fire exposure
Wet-cleaned drape equals retest. Topical FR treatment washes out. If a stage cloth has been laundered without an FR re-bath, it's no longer compliant - even if the tag is still current. The cleaner's docket and the FR cert have to agree.

Quick checks before a show

  • FR tag still legible and inside the recertification window.
  • No visible char, scorch marks, or smoke discolouration.
  • No water staining (water damage compromises topical FR).
  • Seams and webbing intact, no torn grommets at hang points.

If a drape fails any of the above, take it out of service and call us on 1300 439 872. We re-treat and recertify in-house and turn most loads in two to three weeks.